GRAD | Br | Hcb | Hcj | (BH) maximal | ||||
T | GS | KA/m | OE | KA/m | OE | KJ/m3 | MGOe | |
JC-Y3932 | 0.375-0.400 | 3750-4000 | 230-275 | 2890-3456 | 235-290 | 2950-3645 | 26.5-31.5 | 3.33-3.96 |
JC-Y3939 | 0.380-0.400 | 3800-4000 | 255-290 | 3200-3645 | 260-325 | 3260-4080 | 26.5-31.8 | 3.33-4.00 |
JC-Y4041 | 0.390-0.415 | 3900-4150 | 260-300 | 3260-3770 | 300-350 | 3770-4400 | 27.0-32.0 | 3.39-4.02 |
JC-Y4127 | 0.400-0.420 | 4000-4200 | 180-225 | 2260-2825 | 185-228 | 2320-2865 | 30.0-33.6 | 3.77-4.22 |
JC-Y4231 | 0.410-0.430 | 4100-4300 | 220-260 | 2765-3265 | 255-270 | 2825-3390 | 31.5-35.5 | 3.95-4.46 |
JC-Y3849 | 0.370-0.400 | 3700-4000 | 271-305 | 3405-3830 | 370-400 | 4650-5025 | 26.0-31.2 | 3.27-3.92 |
JC-Y4240 | 0.410-0.430 | 4100-4300 | 285-314 | 3580-3945 | 306-340 | 3845-4270 | 31.5-34.4 | 3.95-4.32 |
JC-Y4545 | 0.440-0.460 | 4400-4600 | 310-354 | 3895-4445 | 346-375 | 4350-4710 | 36.5-39.5 | 4.59-4.96 |
JC-Y4350 | 0.420-0.440 | 4200-4400 | 295-325 | 3700-4080 | 382-410 | 4800-5150 | 33.5-36.5 | 4.21-4.59 |
Gemacht von SrO. 6Fe2O3 und andere Mikroelemente durch die keramische Verarbeitung.
Strontiumferritpulver sind entworfen worden, um alle Grade des harten Ferrits zu produzieren. Wir machen hohe Qualität, indem wir richtige Zusätze in die Pulver addieren. Unser strenges Qualitätskontrollsystem garantieren, dass die Qualität stabil und zuverlässig ist.
Produktarten verfügbar: Bogen, Segment, Block